Lincoln OEM - BASE BEZEL - M26000-5 - 9SM26000-5 10n46 low-hydrogen electrodes exposed to atmosphere
Description
low-hydrogen electrodes exposed to atmosphere beyond 4 hours must be rebaked at 500-800 F for 1-2 hours or stored in a heated rod oven at 250-300 F
Oversized square tube legs and braces increase durability and reduce flex under load
9% of UV-A
Lincoln OEM SWITCH & RECEPTACLE ASBLY M17286 - 9SM17286
Lincoln OEM - BASE BEZEL - M26000-5 - 9SM26000-5 10n46 low-hydrogen electrodes exposed to atmosphereLincoln OEM BASE BEZEL M26000 5 9SM26000 5